1Comparison between the effects of ultrasound and γ-rays on the inactivation of Saccharomyces cerevisiae : Analyses of cell membrane permeability and DNA or RNA synthesis by flow cytometry显示文摘Ikuko Oyane Tomo Takeda Yasunori Oda Takashi Sakata Masakazu Furuta Kenji Okitsu Yasuaki Maeda Rokuro Nishimura 2009Ultrasonics - Sonochemistry2009,,4:1
2SCC evaluation of type 304 and 316 austenitic stainless steels in acidic chloride solutions using the slow strain rate technique显示文摘ROKURO N YASUAKI M 2004Corrosion Science2004,46,:1
3The effects of air pollution and climatic factors on atmospheric corrosion of marble under field exposure显示文摘Tran Thi Ngoc Lan Rokuro Nishimura Yoshio Tsujino Yukihiro Satoh Nguyen Thi Phuong Thoa Masayuki Yokoi Yasuaki Maeda 2004Corrosion Science2004,,4:1
4Metal dissolution and maximumstrss during SCC Process of ferritic(type430)and austenitic(type304 and type316) stainless in acidic chlorideSolutions under constant applied stress 显示文摘Rokuro Nishimura Yasuaki Maeda 2004Corrosion science2004,46,76:1
5Volatile components of Artemisia capillaris显示文摘Rokuro Harada Maroka Iwasaki 1982Phytochemistry1982,21,8:1
6The effect of sensitizing temperature on stress corrosion cracking of type 316 austenitic stainless steel in hydrochloric acid solu- tion 显示文摘Rokuro Nishimura Iing Musalam Yasuaki Maeda 2002Corros Sci2002,44,:1
7The effects of air pollution and climatic factors on atmospheric corrosion of marble under field exposure 显示文摘TRAN THIN L ROKURO N TSUJINO Y 2005Corrosion Science2005,47,4:1
8Dimethylehlorosilane and some of its derivatives from the low boiling product of silicon-methylchloride reaction 显示文摘ROKURO O MINORU S 1955Kogyo Kagaku Zasshi1955,58,11:1
9SCC evaluation oftype 304 and 316 austenitic stainless steels inacidic chloride solutions using the slow strain ratetechnique显示文摘ROKURO N YASUAKI M 2004Corrosion Science2004,46,:1
10Stress Corrosion Cracking and Hydrogen Embrittlement of Sensitized Austenitic Stainless Steels in Boiling Saturated Magnesium Chloride Solutions 显示文摘Osama M Alyousif Rokuro Nishimura 2008Corrosion Science2008,50,:1
11Characterization and perspective of stress corrosion cracking of austenitic stainless steels( type 304 and type316) in acid solutions using constant load method显示文摘Rokuro Nishimura 2007Corrosion Science2007,49,:1
12On the stress corrosion cracking and hydrogen embrittlement of sensitized austenitic stain- less steels in boiling saturated magnesium chloride solutions: Effect of applied stress 显示文摘Osama M Alyousif Rokuro Nishimura 2008Corrosion Science2008,,50:1
13The effect of sensitizing temperature on stress corrosion cracking of type 316L austenitic stainless steel in hydrochloric acid solution 显示文摘Rokuro Nishimura Ling Musalam Yasuaki Maeda 2002Corrosion Science2002,44,:1
14Synthesis and structure-activity relatlon-shlps of a novel nral carbapenem, CS-834 显示文摘MASAO M ROKURO E MASAFUMI H 1997J Antibiotics1997,50,5:1
15SCC evaluation of type 304 and 316 austenitic of type 304 and 316 austenitic stainless steels in acidic chloride solutions using the slow strain rate technique 显示文摘Rokuro N Yasuaki M 2004Corrosion Science2004,,46:1
16Stress corrosion cracking of type 304austenitic stainless steel in sulphuric acid solution including sodium chloride and chromate 显示文摘Rokuro Nishimura Yasuaki Maeda 2004Corrosion Science2004,46,2:1
17On the Stress Corrosion Cracking and Hydrogen Embrittlement of SOnsitized Austenitic Stainless Steels in Boiling Saturated Magnesium Chloride Solutions:Effect of Applied Stress显示文摘Osama M Myousif Rokuro Nishimura 2008Corrosion Science2008,50,:1
18Separation of scandium and rare earths by anion exchange in acetic acid-HC1 mixtures显示文摘ROKURO K IKUKO H 1966Journal of Chromatorgraphy1966,25,:1
19On the Stress Corrosion Cracking and Hydrogen Embrittlement of Sensitized Austenitic Stainless Steels in Boiling Saturated Magnesium Chloride Solutions: Effect of Applied Stress 显示文摘Osama M Alyousif Rokuro Nishimura 2008Corrosion Science2008,50,:1
20SCC Evaluation of Type 304 and 316 Austenitie of Type 304 and 316 Austenitie Stainless Steels in Acidic Chloride Solutions Using the Slow Strain Rate Technique 显示文摘Rokuro Nishimura Yasuaki Maeda 2004Corrosion Science2004,46,:1
返回顶部 每页显示:
共3页 首页 上一页 第1页 下一页 末页 /3 跳转

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费